Galvanic corrosion, a type of electrochemical corrosion, can cause significant damage to metals when two different metals are in electrical contact and immersed in an electrolyte. This occurs due to the creation of a galvanic couple, where one metal acts as an anode and the other as a cathode, leading to accelerated corrosion of the anode. To prevent and mitigate such damage, it's crucial to understand and test for galvanic corrosion. Here, we delve into the intricacies of galvanic corrosion and provide a comprehensive guide on how to test for it.

Galvanic corrosion often goes unnoticed until it's too late, making preventive testing essential. It can lead to system failures, expensive repairs, and even safety hazards. By understanding the factors that contribute to galvanic corrosion and knowing how to test for it, you can extend the lifespan of your metal structures and equipment.

Understanding Galvanic Corrosion

Before discussing how to test for galvanic corrosion, it's crucial to understand the factors that contribute to its occurrence. These include the types of metals involved, the electrolyte, and the presence of an electrical connection between the metals. The galvanic series, a list of metals ranked by their tendency to act as an anode or cathode, is an essential tool in predicting galvanic corrosion.

Rusting of Iron Diagram | Corrosion, Oxidation and Prevention Explained
Rusting of Iron Diagram | Corrosion, Oxidation and Prevention Explained
Comprehensive Corrosion Test: 46 Products Compared | Day At The Range
Comprehensive Corrosion Test: 46 Products Compared | Day At The Range
Everything architects need to know about Galvanic Corrosion (and a Mnemonic Device to you remember it)
Everything architects need to know about Galvanic Corrosion (and a Mnemonic Device to you remember it)

The potential difference between two metals in the galvanic series can indicate the likelihood and severity of galvanic corrosion. A large potential difference increases the corrosion risk. For instance, stainless steel and aluminum have a significant potential difference, making them a poor combination when electrically connected in the presence of an electrolyte.

Galvanic Series

The galvanic series is divided into two parts: the series Noble Metals (anodic to cathodic) and the series Active Metals (cathodic to anodic). In the Noble Metals part, the metals with the most noble behavior, like gold, are at the top, while materials with active behavior, such as magnesium alloys, are at the bottom of the Active Metals part. Understanding the galvanic series can help you make informed decisions when selecting materials to use together.

the diagram shows how to remove rust with electrolysiss and other things that are necessary
the diagram shows how to remove rust with electrolysiss and other things that are necessary
Understand galvanic corrosion and how it affects screws in your projects with galvanic reaction chart! Contact us for expert advice on preventing corrosion! #engineeringedge #eesg #corroshield #tapperman #dyno #learnmore #engineeringbasics #fasteners #corrosion Engineering
Understand galvanic corrosion and how it affects screws in your projects with galvanic reaction chart! Contact us for expert advice on preventing corrosion! #engineeringedge #eesg #corroshield #tapperman #dyno #learnmore #engineeringbasics #fasteners #corrosion Engineering
Types of Corrosion | Common Forms of Corrosion
Types of Corrosion | Common Forms of Corrosion

Example of Galvanic Series:

  • Gold, Silver
  • Tin
  • Lead, Nickel, Copper
  • Brass (70-30), Bronze
  • Aluminum, Mild Steel, Cast Iron
  • Silver solder, Solders
  • Zinc, Galvanized Iron
  • Magnesium, Magnesium Alloys

Electrolyte and Electrical Connection

The electrolyte, a conductive solution that acts as a bridge between the two metals, plays a significant role in galvanic corrosion. Electrolytes can be found in various forms, such as water, soil, or even moisture in the air. The electrical connection between the two metals, which can be intentional (like in electrical systems) or unintentional (due to poor grounding or touchpoints), completes the galvanic couple.

Tarnish and Corrosion
Tarnish and Corrosion
an image of the structure of water and other things in which it is important to float
an image of the structure of water and other things in which it is important to float
Understand galvanic corrosion and how it affects screws in your projects with galvanic reaction chart! Contact us for expert advice on preventing corrosion! #engineeringedge #eesg #corroshield #tapperman #dyno #learnmore #engineeringbasics #fasteners #corrosion Corrosion Vs Oxidation Comparison Chart, Galvanic Corrosion Chart Metals, Galvanic Corrosion Diagram, Metal Corrosion Chart, Metal Corrosion Rates Chart, Galvanic Corrosion Chart, Galvanic Corrosion Table, Metal Corrosion Comparison, Types Of Corrosion
Understand galvanic corrosion and how it affects screws in your projects with galvanic reaction chart! Contact us for expert advice on preventing corrosion! #engineeringedge #eesg #corroshield #tapperman #dyno #learnmore #engineeringbasics #fasteners #corrosion Corrosion Vs Oxidation Comparison Chart, Galvanic Corrosion Chart Metals, Galvanic Corrosion Diagram, Metal Corrosion Chart, Metal Corrosion Rates Chart, Galvanic Corrosion Chart, Galvanic Corrosion Table, Metal Corrosion Comparison, Types Of Corrosion
Understand galvanic corrosion and how it affects screws in your projects with galvanic reaction chart! Contact us for expert advice on preventing corrosion! #engineeringedge #eesg #corroshield #tapperman #dyno #learnmore #engineeringbasics #fasteners #corrosion Repair, Engineering, Things To Come
Understand galvanic corrosion and how it affects screws in your projects with galvanic reaction chart! Contact us for expert advice on preventing corrosion! #engineeringedge #eesg #corroshield #tapperman #dyno #learnmore #engineeringbasics #fasteners #corrosion Repair, Engineering, Things To Come
an orange and yellow line with the words galvaniic scale
an orange and yellow line with the words galvaniic scale
Keep Corrosion at Bay | Cruising World
Keep Corrosion at Bay | Cruising World

Example of Electrolyte and Electrical Connection:

ElectrolyteExample
Natural WaterSeawater, Freshwater, Rainwater
SoilMoist Soils, Saline Soils
Moisture in AirCondensation, Humidity

Testing for Galvanic Corrosion

Once you understand the fundamentals of galvanic corrosion, you can perform various tests to identify potential issues and mitigate risks. These tests mainly involve monitoring electrical potentials, measuring corrosion rates, and visual inspections.

Corrosion and Rusting Lab Activities ⋆ iTeachly.com
Corrosion and Rusting Lab Activities ⋆ iTeachly.com
Understand galvanic corrosion and how it affects screws in your projects with galvanic reaction chart! Contact us for expert advice on preventing corrosion! #engineeringedge #eesg #corroshield #tapperman #dyno #learnmore #engineeringbasics #fasteners #corrosion Electrolyte Water, Engineering, Instagram
Understand galvanic corrosion and how it affects screws in your projects with galvanic reaction chart! Contact us for expert advice on preventing corrosion! #engineeringedge #eesg #corroshield #tapperman #dyno #learnmore #engineeringbasics #fasteners #corrosion Electrolyte Water, Engineering, Instagram
Galvanic Corrosion Chart and Calculator
Galvanic Corrosion Chart and Calculator

Regular testing can help you maintain your equipment's integrity, extend its lifespan, and prevent unexpected failures. It's recommended to test metal structures and equipment regularly, especially in harsh environments or where galvanic corrosion is likely to occur.

Potential Difference Measurements

Measuring the potential difference between two metals can help identify if a galvanic couple exists. Using a high-impedance voltmeter, measure the open-circuit potential (OCP) of each metal in the electrolyte. If the potential difference is significant, it indicates that galvanic corrosion may occur.

To mitigate galvanic corrosion, you can either:

  • Use suitable metals that have a small potential difference (ideally, less than 0.1 V).
  • Prevent electrical contact between the metals, or
  • Use protective measures, such as cathodic protection or protective coatings.

Corrosion Rate Measurements

Corrosion rate measurements provide a direct indicator of the corrosion activity. Techniques like linear polarization resistance (LPR), electrochemical impedance spectroscopy (EIS), and weight loss measurements can be employed to determine the corrosion rate.

Once you've identified a high corrosion rate, you can implement mitigation strategies, such as:

  • Isolating the metals to break the electrical connection.
  • Using inhibitors to slow down the corrosion process.
  • Applying protective coatings to physically separate the metal from the electrolyte.
  • Implementing cathodic protection to shift the potential of the anode to more noble values.

Regularly testing your metal structures and equipment for galvanic corrosion ensures their longevity and safety. It's a proactive approach to maintenance that can save you time, money, and resources in the long run. By understanding and testing for galvanic corrosion, you can make informed decisions and create robust maintenance plans.